护壁泥浆对灌浆水泥的劣化机理及抗污染优化
CSTR:
作者:
作者单位:

1中国水利水电第七工程局成都水电建设工程有限公司,四川 成都 610213;2地质灾害防治与地质环境保护全国重点实验室,四川 成都 610059

作者简介:

通讯作者:

中图分类号:

P634;TV543

基金项目:

中国水利水电第七工程局有限公司科技项目(编号:2025-1020-95-45)


Deterioration mechanism of grouting cement induced by wall-protecting mud and anti-contamination optimization
Author:
Affiliation:

1Chengdu Hydropower Construction Engineering Co., Ltd. of China Water Resources and Hydropower Seventh Engineering Bureau, Chengdu Sichuan 610213, China;2State Key Laboratory of Geohazard Prevention and Geoenvironment Protection, Chengdu Sichuan 610059, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    针对西南深山峡谷地区水电站建设工程中护壁泥浆残留与水泥浆接触污染导致胶结面强度弱化、灌浆质量下降的问题,通过室内试验,研究3种典型护壁泥浆与水泥净浆以不同体积比混合后的接触污染效应,测试了混合浆体的流动度、凝结时间及不同龄期抗压强度,并结合扫描电镜微观分析,揭示了泥浆对灌浆水泥的性能劣化规律及作用机理。结果表明:泥浆残留显著劣化水泥净浆性能,膨润土基泥浆主要通过颗粒包裹层抑制水化并诱发干缩裂隙;黄原胶无固相泥浆因有机?无机界面脱黏导致结构崩解,20%掺量时1 d强度损失率高达93.8%,且完全丧失可泵性。基于此,通过外加剂筛选与正交试验,优选出水灰比0.4、掺入0.1%减水剂、0.25%早强剂及0.55%纳米二氧化硅的高性能抗污染灌浆配方,其可泵期达80 min,终凝时间180 min。该优化配方1 d强度达18.8 MPa,较普通净浆提升10倍以上,流动度26.0 cm;在泥浆污染环境下,力学性能提升幅度显著,有效抵抗了水化抑制与收缩破裂,显著增强了抗泥浆污染能力,为复杂地层灌浆施工提供了理论依据与技术支撑。

    Abstract:

    To address the problems of cementation strength weakening and grouting quality deterioration caused by contact contamination between residual wall-protecting mud and cement slurry during hydropower station construction in deep mountain and canyon areas of Southwest China, laboratory tests were conducted to investigate the contact contamination effects of three typical wall-protecting muds mixed with neat cement paste at different volume ratios. The fluidity, setting time, and compressive strength at different ages of the mixed slurries were tested, and scanning electron microscopy (SEM) microanalysis was performed to reveal the deterioration patterns and mechanisms of mud on the performance of grouting cement. The results show that mud residue significantly deteriorates the performance of neat cement paste. Bentonite-based muds primarily inhibit hydration and induce drying shrinkage cracks through particle coating layers, while xanthan gum non-solid-phase mud causes structural disintegration due to organic-inorganic interface debonding. At a 20% mixing ratio, the 1-day strength loss rate of the latter reaches as high as 93.8%, with a complete loss of pumpability. Based on these findings, through admixture screening and orthogonal tests, a high-performance anti-contamination grouting formulation was optimized with a water-cement ratio of 0.4, incorporating 0.1% superplasticizer, 0.25% early-strength agent, and 0.55% nano-silica. Its pumpable period reaches 80 min, and the final setting time is 180 min. This optimized formulation achieves a 1-day strength of 18.8 MPa, which is more than 10 times higher than that of ordinary neat cement paste, along with a fluidity of 26.0 cm. Under mud contamination conditions, its mechanical properties are significantly improved, effectively resisting hydration inhibition and shrinkage cracking, and markedly enhancing the anti-mud contamination capability. This study provides a theoretical basis and technical support for grouting construction in complex strata.

    参考文献
    相似文献
    引证文献
引用本文

李建,杨康,高自全,等.护壁泥浆对灌浆水泥的劣化机理及抗污染优化[J].钻探工程,2026,53(6):127-137.
LI Jian, YANG Kang, GAO Ziquan, et al. Deterioration mechanism of grouting cement induced by wall-protecting mud and anti-contamination optimization[J]. Drilling Engineering, 2026,53(6):127-137.

复制
分享
相关视频

文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2026-03-23
  • 最后修改日期:2026-04-28
  • 录用日期:2026-05-09
  • 在线发布日期: 2026-11-27
  • 出版日期: 2026-11-10
文章二维码